Formulas · free calculator
Minimum inside radius by material and temper
The tightest radius before the outside face cracks.
Mild steel, Annealed = 0.5 × T
Minimum inside radius = 1 mm
Radius 3 mm is inside the limit.
Table values, nominal thickness. Values are a starting point — press rating, die condition, material certificate and grain direction move the real number.
Have the actual STEP file measured against these limits — first part freeThe rule
Minimum inside radius = factor × T, per material and temper. Galvanized and hard tempers need more.
Radius is a material property before it is a design choice. Below the limit the part cracks with no warning.
What breaks when this is ignored
- A 1 × T radius specified on 6061-T6 — that is a 4 × T material.
- Bending across the grain when the part allows bending along it.
- A radius under 1 × T quoted as an air bend; it needs coining or bottoming and the tooling priced.
Minimum radius, multiple of thickness
| Material | Annealed | 1/4 hard | 1/2 hard | Hard |
|---|---|---|---|---|
| Mild steel | 0.5 T | 1 T | 1.5 T | 2 T |
| Aluminium 5052 | 0.5 T | 1 T | 1.5 T | 2.5 T |
| Aluminium 6061 | 1 T | 2 T | 3 T | 4 T |
| Stainless 304 | 1 T | 1.5 T | 2 T | 3 T |
Notes from the floor
- Galvanized carries 1.5 T across the board because the zinc flakes before the steel yields.
All eight formulas on paper
The Press Brake Reference prints every table with the arithmetic worked, plus ten field notes. CA$29, PDF.